Laminate reference
Shengyi SF201
εᵣ 3.2 · Df 0.008
Single-sided adhesiveless polyimide FCCL. Dk 3.2 / Df 0.008 at 1 MHz (12.5 µm constructions). No Tg published.
- Manufacturer
- Shengyi
- Dielectric constant εᵣ
- 3.2
- Dissipation factor Df
- 0.008
- Glass transition Tg
- Unconfirmed
- Categories
- Flex / rigid-flex
- Dk basis
- Datasheet
- Df basis
- Datasheet
- Dk / Df measured at
- 1 MHz, C-24/23/50
- Bonding method
- Separate bondply required
Cores
Dielectric thickness of the laminate alone, and the finished core with copper on both faces.
| Designation | Dielectric | +2 × 0.5 oz | +2 × 1 oz | +2 × 2 oz |
|---|---|---|---|---|
| SF201-0512SE | 0.013 mm | 0.049 mm | 0.083 mm | 0.153 mm |
| SF201-0512SR | 0.013 mm | 0.049 mm | 0.083 mm | 0.153 mm |
| SF201-0518SE | 0.013 mm | 0.049 mm | 0.083 mm | 0.153 mm |
| SF201-0518SR | 0.013 mm | 0.049 mm | 0.083 mm | 0.153 mm |
| SF201-0812SE | 0.020 mm | 0.056 mm | 0.090 mm | 0.160 mm |
| SF201-0812SR | 0.020 mm | 0.056 mm | 0.090 mm | 0.160 mm |
| SF201-0818SE | 0.020 mm | 0.056 mm | 0.090 mm | 0.160 mm |
| SF201-0818SR | 0.020 mm | 0.056 mm | 0.090 mm | 0.160 mm |
Typical values from manufacturer datasheets and IPC-4101 nominals, at the frequency the manufacturer publishes. Confirm the exact grade, glass style and pressed thickness with your fabricator.
Related laminates
Build a stack-up on SF201
Create a free account, pick SF201 as the material system on Requirements, and PCB Starting Point generates candidate constructions from these exact thicknesses, sizes impedance traces on its εᵣ and checks the build against fabrication rules.