PCB Starting Point

Laminate reference

Rogers ULTRALAM 3850HT

εᵣ 2.9 · Df 0.002

High-temperature LCP clad. Melts at about 335°C; no Tg. Bond with ULTRALAM 3908 LCP bondply.

Manufacturer
Rogers
Dielectric constant εᵣ
2.9
Dissipation factor Df
0.002
Glass transition Tg
Not applicable
Categories
Flex / rigid-flex, RF / microwave
Dk basis
Published typical
Df basis
Published typical
Bonding method
Manufacturer-specific bonding system

Cores

Dielectric thickness of the laminate alone, and the finished core with copper on both faces.

DesignationDielectric+2 × 0.5 oz+2 × 1 oz+2 × 2 oz
LCP3850HT-25/180.025 mm0.061 mm0.095 mm0.165 mm
LCP3850HT-50/180.050 mm0.086 mm0.120 mm0.190 mm
LCP3850HT-100/180.100 mm0.136 mm0.170 mm0.240 mm

Other forms

DesignationTypeDielectricNotes
LCP3850HT-25umFilm0.025 mmLCP, higher thermal reliability than 3850
LCP3850HT-50umFilm0.050 mmLCP
LCP3850HT-100umFilm0.100 mmLCP
LCP3850HT-3908-0.025Bondply0.025 mmULTRALAM 3908 LCP bondply
LCP3850HT-3908-0.050Bondply0.050 mmULTRALAM 3908 LCP bondply

Typical values from manufacturer datasheets and IPC-4101 nominals, at the frequency the manufacturer publishes. Confirm the exact grade, glass style and pressed thickness with your fabricator.