Isola I-Speed

εᵣ 3.63 · Df 0.006 · Tg 180 °C

180°C Tg FR-4 for high speed. Tg 180°C DSC, 195°C DMA. All glass is spread weave. Prepreg from Isola's table at 10 GHz, the lowest resin content of each glass style.

厂商
Isola
介电常数 εᵣ
3.63
损耗因子 Df
0.006
玻璃化转变温度 Tg
180 °C
类别
高速 / 低损耗
Dk 依据
数据表
Df 依据
数据表
Dk / Df 测试频率
10 GHz
1 GHz 下的 Dk / Df
3.65 / 0.006
热分解温度 Td
360 °C
Z 轴 CTE
45 ppm/°C before Tg, 230 ppm/°C after Tg
X / Y 向 CTE
16 ppm/°C
IPC-4101
/98 /99 /101 /126
无铅
是

半固化片

按玻纤布型号列出的每张压合后厚度。

型号玻纤布介质备注
I-Speed-106710670.051 mm
I-Speed-103510350.061 mm
I-Speed-108010800.079 mmMost common thin PP
I-Speed-108610860.084 mm
I-Speed-107810780.091 mm
I-Speed-331333130.102 mmMedium, spread glass
I-Speed-211621160.130 mmStandard build-up

芯板

仅板材本身的介质厚度,以及双面覆铜后的成品芯板厚度。

型号介质+2 × 0.5 oz+2 × 1 oz+2 × 2 oz
I-Speed-0.050.050 mm0.086 mm0.120 mm0.190 mm
I-Speed-0.100.100 mm0.136 mm0.170 mm0.240 mm
I-Speed-0.150.150 mm0.186 mm0.220 mm0.290 mm
I-Speed-0.200.200 mm0.236 mm0.270 mm0.340 mm
I-Speed-0.250.250 mm0.286 mm0.320 mm0.390 mm
I-Speed-0.300.300 mm0.336 mm0.370 mm0.440 mm
I-Speed-0.350.350 mm0.386 mm0.420 mm0.490 mm
I-Speed-0.400.400 mm0.436 mm0.470 mm0.540 mm
I-Speed-0.500.500 mm0.536 mm0.570 mm0.640 mm
I-Speed-0.710.710 mm0.746 mm0.780 mm0.850 mm
I-Speed-1.001.000 mm1.036 mm1.070 mm1.140 mm
I-Speed-1.201.200 mm1.236 mm1.270 mm1.340 mm
I-Speed-1.501.500 mm1.536 mm1.570 mm1.640 mm
I-Speed-1.551.550 mm1.586 mm1.620 mm1.690 mm

典型值来自厂商规格书和 IPC-4101 标称值,取厂商公布的频率。请与板厂确认具体等级、玻纤布型号和压合后厚度。