Laminate reference
TUC ThunderClad 1 (TU-863)
εᵣ 3.9 · Df 0.01 · Tg 180 °C
High-Tg halogen-free low loss. Tg 180°C DSC, 170°C TMA, 210°C DMA. At 1 GHz: 4.1 / 0.008 (SPC) and 3.9 / 0.006 (HP4291B).
- Manufacturer
- TUC
- Dielectric constant εᵣ
- 3.9
- Dissipation factor Df
- 0.01
- Glass transition Tg
- 180 °C
- Categories
- Halogen-free, High-Tg / reliability, High-speed / low-loss
- Dk basis
- Datasheet
- Df basis
- Datasheet
- Dk / Df measured at
- 10 GHz, 50% resin
- Decomposition Td
- 365 °C
- Z-axis CTE
- 2.6% from 50 to 260°C
- IPC-4101
- /127 /128 /130
- Halogen-free
- Yes
- Lead-free
- Yes
Prepregs
Pressed thickness per ply by glass style.
| Designation | Glass | Dielectric | Notes |
|---|---|---|---|
| TU863-106 | 106 | 0.050 mm | High resin, thin |
| TU863-1080 | 1080 | 0.075 mm | Most common thin PP |
| TU863-2113 | 2113 | 0.095 mm | Medium |
| TU863-2116 | 2116 | 0.115 mm | Standard build-up |
| TU863-1506 | 1506 | 0.165 mm | Thicker filler |
| TU863-7628 | 7628 | 0.195 mm | Thick / cost effective |
Cores
Dielectric thickness of the laminate alone, and the finished core with copper on both faces.
| Designation | Dielectric | +2 × 0.5 oz | +2 × 1 oz | +2 × 2 oz |
|---|---|---|---|---|
| TU863-0.05 | 0.050 mm | 0.086 mm | 0.120 mm | 0.190 mm |
| TU863-0.10 | 0.100 mm | 0.136 mm | 0.170 mm | 0.240 mm |
| TU863-0.15 | 0.150 mm | 0.186 mm | 0.220 mm | 0.290 mm |
| TU863-0.20 | 0.200 mm | 0.236 mm | 0.270 mm | 0.340 mm |
| TU863-0.25 | 0.250 mm | 0.286 mm | 0.320 mm | 0.390 mm |
| TU863-0.30 | 0.300 mm | 0.336 mm | 0.370 mm | 0.440 mm |
| TU863-0.35 | 0.350 mm | 0.386 mm | 0.420 mm | 0.490 mm |
| TU863-0.40 | 0.400 mm | 0.436 mm | 0.470 mm | 0.540 mm |
| TU863-0.50 | 0.500 mm | 0.536 mm | 0.570 mm | 0.640 mm |
| TU863-0.71 | 0.710 mm | 0.746 mm | 0.780 mm | 0.850 mm |
| TU863-1.00 | 1.000 mm | 1.036 mm | 1.070 mm | 1.140 mm |
| TU863-1.20 | 1.200 mm | 1.236 mm | 1.270 mm | 1.340 mm |
| TU863-1.50 | 1.500 mm | 1.536 mm | 1.570 mm | 1.640 mm |
| TU863-1.55 | 1.550 mm | 1.586 mm | 1.620 mm | 1.690 mm |
Typical values from manufacturer datasheets and IPC-4101 nominals, at the frequency the manufacturer publishes. Confirm the exact grade, glass style and pressed thickness with your fabricator.
Related laminates
Build a stack-up on ThunderClad 1 (TU-863)
Create a free account, pick ThunderClad 1 (TU-863) as the material system on Requirements, and PCB Starting Point generates candidate constructions from these exact thicknesses, sizes impedance traces on its εᵣ and checks the build against fabrication rules.