Laminate reference
Taconic TSM-DS3
εᵣ 3 · Df 0.001
Ceramic-filled, about 5% glass, dimensionally stable. Dk 3.00 ±0.05 (frequency not stated); Df 0.0014 at 10 GHz.
- Manufacturer
- Taconic
- Dielectric constant εᵣ
- 3
- Dissipation factor Df
- 0.001
- Glass transition Tg
- Not applicable
- Categories
- RF / microwave
- Dk basis
- Datasheet
- Df basis
- Datasheet
- Dk / Df measured at
- 10 GHz
- Decomposition Td
- 551 °C
Cores
Dielectric thickness of the laminate alone, and the finished core with copper on both faces.
| Designation | Dielectric | +2 × 0.5 oz | +2 × 1 oz | +2 × 2 oz |
|---|---|---|---|---|
| TSMDS3-0.13 | 0.127 mm | 0.163 mm | 0.197 mm | 0.267 mm |
| TSMDS3-0.25 | 0.254 mm | 0.290 mm | 0.324 mm | 0.394 mm |
| TSMDS3-0.51 | 0.508 mm | 0.544 mm | 0.578 mm | 0.648 mm |
| TSMDS3-0.76 | 0.762 mm | 0.798 mm | 0.832 mm | 0.902 mm |
| TSMDS3-1.52 | 1.524 mm | 1.560 mm | 1.594 mm | 1.664 mm |
| TSMDS3-2.29 | 2.286 mm | 2.322 mm | 2.356 mm | 2.426 mm |
Typical values from manufacturer datasheets and IPC-4101 nominals, at the frequency the manufacturer publishes. Confirm the exact grade, glass style and pressed thickness with your fabricator.
Related laminates
Build a stack-up on TSM-DS3
Create a free account, pick TSM-DS3 as the material system on Requirements, and PCB Starting Point generates candidate constructions from these exact thicknesses, sizes impedance traces on its εᵣ and checks the build against fabrication rules.