PCB Starting Point

Laminate reference

Panasonic Megtron 8

εᵣ 3.13 · Df 0.002 · Tg 220 °C

R-5795(N): Dk 3.13 / Df 0.0016 at 14 GHz; (U) grade 3.08 / 0.0012. Tg 220°C is DMA; Panasonic publishes no DSC or 1 GHz values. Prepreg R-5690.

Manufacturer
Panasonic
Dielectric constant εᵣ
3.13
Dissipation factor Df
0.002
Glass transition Tg
220 °C
Categories
High-speed / low-loss
Dk basis
Datasheet
Df basis
Datasheet

Prepregs

Pressed thickness per ply by glass style.

DesignationGlassDielectricNotes
Meg8-1061060.050 mmHigh resin, thin
Meg8-108010800.075 mmMost common thin PP
Meg8-211321130.095 mmMedium
Meg8-211621160.115 mmStandard build-up
Meg8-150615060.165 mmThicker filler
Meg8-762876280.195 mmThick / cost effective

Cores

Dielectric thickness of the laminate alone, and the finished core with copper on both faces.

DesignationDielectric+2 × 0.5 oz+2 × 1 oz+2 × 2 oz
Meg8-0.050.050 mm0.086 mm0.120 mm0.190 mm
Meg8-0.100.100 mm0.136 mm0.170 mm0.240 mm
Meg8-0.150.150 mm0.186 mm0.220 mm0.290 mm
Meg8-0.200.200 mm0.236 mm0.270 mm0.340 mm
Meg8-0.250.250 mm0.286 mm0.320 mm0.390 mm
Meg8-0.300.300 mm0.336 mm0.370 mm0.440 mm
Meg8-0.350.350 mm0.386 mm0.420 mm0.490 mm
Meg8-0.400.400 mm0.436 mm0.470 mm0.540 mm
Meg8-0.500.500 mm0.536 mm0.570 mm0.640 mm
Meg8-0.710.710 mm0.746 mm0.780 mm0.850 mm
Meg8-1.001.000 mm1.036 mm1.070 mm1.140 mm
Meg8-1.201.200 mm1.236 mm1.270 mm1.340 mm
Meg8-1.501.500 mm1.536 mm1.570 mm1.640 mm
Meg8-1.551.550 mm1.586 mm1.620 mm1.690 mm

Typical values from manufacturer datasheets and IPC-4101 nominals, at the frequency the manufacturer publishes. Confirm the exact grade, glass style and pressed thickness with your fabricator.

Related laminates

Build a stack-up on Megtron 8

Create a free account, pick Megtron 8 as the material system on Requirements, and PCB Starting Point generates candidate constructions from these exact thicknesses, sizes impedance traces on its εᵣ and checks the build against fabrication rules.