PCB Starting Point

Laminate reference

Kingboard KB-6164

εᵣ 4.6 · Df 0.016 · Tg 140 °C

Lead-free, low Z-CTE, anti-CAF. Dk 4.6 / Df 0.016 at 1 GHz. Prepreg KB-6064 line-up.

Manufacturer
Kingboard
Dielectric constant εᵣ
4.6
Dissipation factor Df
0.016
Glass transition Tg
140 °C
Categories
Standard FR-4
Dk basis
Published typical
Df basis
Published typical

Prepregs

Pressed thickness per ply by glass style.

DesignationGlassDielectricNotes
KB-6164-1061060.050 mmHigh resin, thin
KB-6164-108010800.066 mmMost common thin PP
KB-6164-211621160.117 mmStandard build-up
KB-6164-762876280.185 mmThick / cost effective

Cores

Dielectric thickness of the laminate alone, and the finished core with copper on both faces.

DesignationDielectric+2 × 0.5 oz+2 × 1 oz+2 × 2 oz
KB-6164-0.050.050 mm0.086 mm0.120 mm0.190 mm
KB-6164-0.100.100 mm0.136 mm0.170 mm0.240 mm
KB-6164-0.150.150 mm0.186 mm0.220 mm0.290 mm
KB-6164-0.200.200 mm0.236 mm0.270 mm0.340 mm
KB-6164-0.250.250 mm0.286 mm0.320 mm0.390 mm
KB-6164-0.300.300 mm0.336 mm0.370 mm0.440 mm
KB-6164-0.350.350 mm0.386 mm0.420 mm0.490 mm
KB-6164-0.400.400 mm0.436 mm0.470 mm0.540 mm
KB-6164-0.500.500 mm0.536 mm0.570 mm0.640 mm
KB-6164-0.710.710 mm0.746 mm0.780 mm0.850 mm
KB-6164-1.001.000 mm1.036 mm1.070 mm1.140 mm
KB-6164-1.201.200 mm1.236 mm1.270 mm1.340 mm
KB-6164-1.501.500 mm1.536 mm1.570 mm1.640 mm
KB-6164-1.551.550 mm1.586 mm1.620 mm1.690 mm

Typical values from manufacturer datasheets and IPC-4101 nominals, at the frequency the manufacturer publishes. Confirm the exact grade, glass style and pressed thickness with your fabricator.