PCB Starting Point

Laminate reference

Generic Aluminium IMS

Single-sided aluminium board. Plate plus a thermal dielectric. Circuit copper is the foil.

Manufacturer
Generic IMS
Dielectric constant εᵣ
Not applicable
Dissipation factor Df
Not applicable
Glass transition Tg
Not applicable
Categories
Metal-core / thermal

Prepregs

Pressed thickness per ply by glass style.

DesignationGlassDielectricNotes
Al-1.0W-0.075—0.075 mmThermal dielectric, 1.0 W/m·K, 0.075 mm. Dk 4.8 is typical for this conductivity.
Al-1.0W-0.100—0.100 mmThermal dielectric, 1.0 W/m·K, 0.1 mm. Dk 4.8 is typical for this conductivity.
Al-1.0W-0.150—0.150 mmThermal dielectric, 1.0 W/m·K, 0.15 mm. Dk 4.8 is typical for this conductivity.
Al-1.5W-0.075—0.075 mmThermal dielectric, 1.5 W/m·K, 0.075 mm. Dk 5.2 is typical for this conductivity.
Al-1.5W-0.100—0.100 mmThermal dielectric, 1.5 W/m·K, 0.1 mm. Dk 5.2 is typical for this conductivity.
Al-1.5W-0.150—0.150 mmThermal dielectric, 1.5 W/m·K, 0.15 mm. Dk 5.2 is typical for this conductivity.
Al-2.0W-0.075—0.075 mmThermal dielectric, 2.0 W/m·K, 0.075 mm. Dk 5.8 is typical for this conductivity.
Al-2.0W-0.100—0.100 mmThermal dielectric, 2.0 W/m·K, 0.1 mm. Dk 5.8 is typical for this conductivity.
Al-2.0W-0.125—0.125 mmThermal dielectric, 2.0 W/m·K, 0.125 mm. Dk 5.8 is typical for this conductivity.
Al-2.0W-0.150—0.150 mmThermal dielectric, 2.0 W/m·K, 0.15 mm. Dk 5.8 is typical for this conductivity.
Al-3.0W-0.100—0.100 mmThermal dielectric, 3.0 W/m·K, 0.1 mm. Dk 6.5 is typical for this conductivity.
Al-3.0W-0.150—0.150 mmThermal dielectric, 3.0 W/m·K, 0.15 mm. Dk 6.5 is typical for this conductivity.

Other forms

DesignationTypeDielectricNotes
Al-5052-0.50Metal0.500 mm0.50 mm 5052-H32. Standard IMS alloy.
Al-6061-0.50Metal0.500 mm0.50 mm 6061-T6. Stiffer, used when the plate is machined.
Al-1050-0.50Metal0.500 mm0.50 mm 1050. Higher thermal conductivity, softer.
Al-5052-0.80Metal0.800 mm0.80 mm 5052-H32. Standard IMS alloy.
Al-6061-0.80Metal0.800 mm0.80 mm 6061-T6. Stiffer, used when the plate is machined.
Al-1050-0.80Metal0.800 mm0.80 mm 1050. Higher thermal conductivity, softer.
Al-5052-1.00Metal1.000 mm1.00 mm 5052-H32. Standard IMS alloy.
Al-6061-1.00Metal1.000 mm1.00 mm 6061-T6. Stiffer, used when the plate is machined.
Al-1050-1.00Metal1.000 mm1.00 mm 1050. Higher thermal conductivity, softer.
Al-5052-1.20Metal1.200 mm1.20 mm 5052-H32. Standard IMS alloy.
Al-6061-1.20Metal1.200 mm1.20 mm 6061-T6. Stiffer, used when the plate is machined.
Al-1050-1.20Metal1.200 mm1.20 mm 1050. Higher thermal conductivity, softer.
Al-5052-1.50Metal1.500 mm1.50 mm 5052-H32. Standard IMS alloy.
Al-6061-1.50Metal1.500 mm1.50 mm 6061-T6. Stiffer, used when the plate is machined.
Al-1050-1.50Metal1.500 mm1.50 mm 1050. Higher thermal conductivity, softer.
Al-5052-1.60Metal1.600 mm1.60 mm 5052-H32. Standard IMS alloy.
Al-6061-1.60Metal1.600 mm1.60 mm 6061-T6. Stiffer, used when the plate is machined.
Al-1050-1.60Metal1.600 mm1.60 mm 1050. Higher thermal conductivity, softer.
Al-5052-2.00Metal2.000 mm2.00 mm 5052-H32. Standard IMS alloy.
Al-6061-2.00Metal2.000 mm2.00 mm 6061-T6. Stiffer, used when the plate is machined.
Al-1050-2.00Metal2.000 mm2.00 mm 1050. Higher thermal conductivity, softer.
Al-5052-2.50Metal2.500 mm2.50 mm 5052-H32. Standard IMS alloy.
Al-6061-2.50Metal2.500 mm2.50 mm 6061-T6. Stiffer, used when the plate is machined.
Al-1050-2.50Metal2.500 mm2.50 mm 1050. Higher thermal conductivity, softer.
Al-5052-3.00Metal3.000 mm3.00 mm 5052-H32. Standard IMS alloy.
Al-6061-3.00Metal3.000 mm3.00 mm 6061-T6. Stiffer, used when the plate is machined.
Al-1050-3.00Metal3.000 mm3.00 mm 1050. Higher thermal conductivity, softer.
Al-5052-3.20Metal3.200 mm3.20 mm 5052-H32. Standard IMS alloy.
Al-6061-3.20Metal3.200 mm3.20 mm 6061-T6. Stiffer, used when the plate is machined.
Al-1050-3.20Metal3.200 mm3.20 mm 1050. Higher thermal conductivity, softer.
Al-5052-4.00Metal4.000 mm4.00 mm 5052-H32. Standard IMS alloy.
Al-6061-4.00Metal4.000 mm4.00 mm 6061-T6. Stiffer, used when the plate is machined.
Al-1050-4.00Metal4.000 mm4.00 mm 1050. Higher thermal conductivity, softer.

Typical values from manufacturer datasheets and IPC-4101 nominals, at the frequency the manufacturer publishes. Confirm the exact grade, glass style and pressed thickness with your fabricator.

Related laminates

Build a stack-up on Aluminium IMS

Create a free account, pick Aluminium IMS as the material system on Requirements, and PCB Starting Point generates candidate constructions from these exact thicknesses, sizes impedance traces on its εᵣ and checks the build against fabrication rules.